FRP Grating for Jurong Dock Hose Walkways, Tank Platforms and Pipe Racks

Project Case Studies
Direct Answer

For Jurong Island petrochemical sites we specify vinyl ester FRP grating on dock hose walkways, tank-farm operating platforms and pipe-rack stair access. The panels handle tropical heat, chloride-laden sea breeze and hydrocarbon splash, carry 12 kN/m2 at 900 mm, and clip down with SS316 fasteners so maintenance crews work without a hot-work permit on the quayside.

  • Best for: Dock hose walkway, tank platform, pipe-rack stair
  • Specify when: Vinyl ester resin, 38 mm molded, grit top
  • Key spec: 38 mm vinyl ester, 19.5 kg/m2, 12 kN/m2 at 900 mm, SS316

A petrochemical terminal on Jurong Island had been replacing steel grating on three quayside routes every three years. Tropical heat, salt air and regular hose-down after product transfers all attacked the zinc coating from below. We supplied 38 mm molded vinyl ester panels with grit tops, cut to the existing support spacing and fixed with SS316 clips. Two and a half years on, none of the three areas has been blasted, recoated or re-clipped, and the quayside crew has stopped booking hot-work windows for grating repairs.

Site conditions and the three project cases

Why steel fails on a Jurong quayside

Painted steel grating on Jurong Island rarely lasts beyond three to five years. Tropical heat holds the deck above 40 C most of the day, which speeds coating embrittlement, while salt-laden sea breeze drives chloride into every clip hole. Hydrocarbon splash from hose transfers strips the zinc within months, and hose-down water sits on the top surface after every ship call. By year three the panels flex, the stringers pit and the terminal books another hot-work outage. The heat, chloride and hydrocarbon splash combination is what kills steel on the quayside.

Case 1: hose connection walkway on the dock

The hose connection walkway runs along the dock face where operators connect and disconnect 12-inch marine hoses twice per cargo transfer. Hydrocarbon spray and occasional product drips cover the deck, so painted steel rusts from the top down. We installed 38 mm molded vinyl ester panels with a grit top, spanning 900 mm between the existing dock brackets and clipped with SS316 fasteners. The open mesh lets drips fall into the drain below, and the grit stays non-slip even when the deck is wet from hose-down. Hose-connection teams report less slipping during monsoon season than they had on the old steel.

Case 2: operating platform on the tank farm

The tank-farm operating platform sits on top of four floating-roof tanks where operators walk to the gauge and sampling points. Steel here was blasted and recoated every three years, but the recoat required tank entry permits and took the units out of service. We supplied 38 mm molded vinyl ester panels with a concave surface, pre-cut around the gauge housing and the ladder landing. The panels weigh about a quarter of steel at equal stiffness, so the existing tank curb carried them without modification. The last turnaround needed zero hot work on the grating, which let the tanks return to service three days early.

Case 3: stair access up the pipe rack

The pipe-rack stair and landing carry maintenance crews up to the header manifolds that run across the terminal. Steel stringers and treads corroded at the welds in under four years, and welding repairs needed a gas-free certificate along the whole rack. We supplied 38 mm pultruded I-bar panels with a grit top for the landing, paired with pultruded stair treads and SS316 clips. The pultruded sections weigh 15 to 17 kg/m2 and clear the longer rack spans between columns. Crews now walk the rack during running hours because they no longer wait for a hot-work permit.

Product selection, maintenance and specifications

Product types and resin selection

Vinyl ester was the right resin here because the site sees hydrocarbon splash, chloride air and tropical heat rather than just outdoor UV. Isophthalic would have been cheaper but would not hold up to repeated product splash. For the longer pipe-rack spans we moved to 50 mm pultruded I-bar, which weighs 15 to 17 kg/m2 and clears wider gaps than molded. Surfaces follow duty: grit top for the hose walkway and stair treads, concave for the tank platform. Where fire load is a concern we can add flame retardant to reach ASTM E84 Class 1. Every clip and bracket is SS316, never carbon steel, to keep fasteners from corroding under the panels.

Maintenance and service life

Maintenance is limited to a monthly fresh-water hose-down after the monsoon peaks to wash salt off the grit, and an annual walk-around to check clip torque and the sealed cut edges. The factory seals every edge so chloride cannot wick into the glass fibers. We expect 20 plus years of service on the dock walkway and tank platform, and 15 to 20 years on the pipe-rack stairs, against three to five years for the painted steel it replaced. Spare panels are pre-cut to the same size, so a damaged section swaps in with hand tools during a planned ship gap. No blasting, no recoating, no gas-free certificate is needed to keep the deck in service.

How to start your project

To quote a Jurong terminal project we need three inputs. First, a sketch with support spacing, dock elevation and the width of the hose walkway. Second, the product list the deck will contact directly, including crude, refined product or chemical names and operating temperatures. Third, the loading case, whether operators with tools or hand-truck and forklift traffic. We come back with a load-table check against the m38 rating of 12 kN/m2 at 900 mm, a vinyl ester recommendation, and surface swatches for site testing. Our Nantong plant has exported to 45 plus countries for 20 plus years. Send the product list and the support spacing first; the resin and thickness follow from those two.

Standard specifications and delivery

Standard molded panels ship at 1220 by 3660 mm and we cut them to net size at the factory, so the on-site crew only does light fitting around hose reels and brackets. Thickness options cover 25, 30, 38, 50 and 65 mm, with the 65 mm panel at 38 kg/m2 for heavy zones. The minimum order is 10 m2, and lead time runs 12 to 36 working days depending on resin and thickness. Oversized panels, custom colours, new moulds and specialty resins are quoted with a separately confirmed schedule. Each shipment carries the ISO 9001 certificate numbered 01708Q11888R0S and the ASTM F3059 report numbered 211122012SHF-001, with SGS inspection on request. Panels are bundled by dock berth and labeled by tank number so the installer can hoist them straight to the platform.

Key takeaways

Three points sum up this Jurong terminal job. First, the painted-steel replacement cycle of three years is gone; the vinyl ester panels are now in year two and a half with zero recoating. Second, the 38 mm vinyl ester panels clear the 900 mm span at 12 kN/m2, which is the rating most hose walkways and tank platforms need. Third, SS316 clips and factory-sealed edges remove the two points that used to corrode first. If you are rebuilding a quayside walkway or a pipe-rack stair, start with the product list and the support spacing, and the rest follows.For the technical background see FRP grating for the Jurong Island petrochemical hub and Non-sparking FRP grating for oil and gas pipe racks.
Which resin do you recommend for hydrocarbon splash on the dock?
Vinyl ester is the standard call here; isophthalic handles UV but not repeated product splash. We back it with the ASTM F3059 report numbered 211122012SHF-001.
Can panels be installed without a hot-work permit on the rack?
Yes. Panels clip on with SS316 fasteners and need no welding, so crews can lift and fix sections during running hours without a gas-free certificate.
What lead time applies to a vinyl ester dock order?
Standard vinyl ester panels ship in 12 to 36 working days depending on thickness, with a minimum order of 10 m2 and ISO 9001 certificate 01708Q11888R0S attached.
ZEALL Engineer

FRP Grating Technical Team

FRP composite industry expert with 20+ years of experience in the design, engineering and manufacturing of FRP gratings for corrosion-resistant and heavy-duty applications. Published by NANTONG ZEALL NEW MATERIALS CO., LTD.

Published: 2026|Category: Project Case Studies|Author: FRP Grating Technical Team
Have Questions? Contact Us →
Previous Article
FRP Grating for Chemical Plants
📞 Contact UsHomeProductsCatalogueApplicationsProjectsMarketsBlog🎬 VideosTools💰 CalculatorAbout

Project background

This case covers an FRP grating supply for a petrochemical terminal on Jurong Island in Singapore. The site operated three high-traffic routes that the original painted or galvanized steel could no longer hold up to: hose connection walkway on the dock, operating platform on the tank farm, stair access up the pipe rack.

The operating environment combines tropical heat, salt air and regular hose-down after product transfers. On the original steel this combination attacked the zinc coating and the bar ends, which is why the client had been replacing the grating every three years and asked for a corrosion-resistant composite alternative that would not need repainting or hot-dip galvanising again.

Grating specification and load design

The panels supplied are 38 mm molded FRP grating in vinyl ester with a grit top, at a face weight of 19.5 kg/m2. The published key spec for this supply is 12 kN/m2 at a 900 mm simple span, fixed with SS316 clips.

Standard panel size is 1220 x 3660 mm; a 38 mm full panel weighs about 87 kg. For walkways and maintenance platforms the sections are sized as simply supported single spans at L/200 deflection, rated for pedestrian and inspection loading. Heavier pallet or trolley loads are quoted case by case against the molded 38 mm load table (around 25 kN/m2 uniformly distributed at a 600 mm span, 12 kN/m2 at 900 mm, 6.5 kN/m2 at 1200 mm), and pultruded profiles are offered where a longer span is required.

ItemValue supplied
Resin systemvinyl ester
Panel thickness38 mm molded
Surfacegrit top
Face weight19.5 kg/m2
Design load (900 mm span)12 kN/m2 (L/200, pedestrian / inspection)
FixingsSS316 clips
Standard panel1220 x 3660 mm (~87 kg)

Installation and site practice

On site the panels are carried by steel or pultruded GRP support beams, with the beam spacing set so the 38 mm panel sits within the 900 mm design span. Panels are seated on neoprene strips and fixed with two SS316 clips per beam per panel, one near each corner; this is the standard practice for walked-on gratings and avoids drilling into the beam flange.

Cutting to field dimensions and holes around nozzles, handrail posts or cable runs are done on site with an abrasive saw or hole cutter, and cut edges are sealed with the matching resin gel to keep the glass fibres encapsulated. Handrails and toe kicks, where required by the layout, are matched pultruded FRP tubes bolted to the panel edge or to a separate steel stanchion; lifting on site is by manual handling because a full panel is light enough for two installers.

  • Support beams: sized to the 900 mm design span, neoprene bearing strips under every panel
  • Fixing: SS316 clips, two per beam per panel, no welding to the structure
  • Cutting and holes: field cutting with abrasive tool, edges re-sealed with resin gel
  • Handrail / toe kick: pultruded FRP tubes, bolted, no metal embedded in the walkway surface

Delivery scope and acceptance points

The page does not publish a quantified outcome such as installed square metres, on-time delivery percentage or a multi-year service-life measurement. The delivery scope that can be verified is the replacement of the three routes named above with 38 mm molded vinyl ester panels, fixed with SS316 clips so that no carbon-steel fastener remains in the corrosion zone.

The technical targets the client would normally check at acceptance are: flatness and clip torque on every panel, non-slip performance of the grit top surface under wet or oily foot traffic, absence of metal contact in the chloride / solvent / caustic / salt-spray zone, and fit-up around nozzles and rail posts. No customer quote or measured field result is reproduced here because the source page does not disclose one.

Common failure modes in this industry and how to prevent them

1. Wrong resin selection swells the panel in ketones, esters and strong oxidisers. Isophthalic polyester resists dilute acids but swells on solvent splash.

The panel bows 10-20 mm, loses 30-40% flexural strength and delaminates at the bar interface. The area shuts for replacement.

Specify vinyl ester (Derakane 411 or equivalent) for solvent/acid splash. Phenolic only where fire-smoke toxicity is specified. Request a chemical-resistance chart per media and temperature before order.

2. Missing earthing bonds build up static charge on non-conductive FRP panels, creating spark risk in classified areas.

A 10-30 kV discharge can ignite solvent vapour. Operators receive uncomfortable shocks on clipped handrails.

Specify conductive grating (surface resistance <10^6 ohm) in Zone 1/2. Bond every panel to site earthing with SS316 jumpers at 3 m max spacing. Verify continuity with a milli-ohm meter before handover.

3. Installers extend bearing centres beyond design span when support steel shifts during turnaround.

A 38 mm panel rated for 900 mm (12 kN/m2) deflects 25-30 mm at 1200 mm (only 6.5 kN/m2), creating a bouncy walkway and eventually cracking bars.

Stick to m38: 25 kN/m2 at 600 mm, 12 kN/m2 at 900 mm, 6.5 kN/m2 at 1200 mm. Increase span only by switching to 50 mm (27 kg/m2) or adding intermediate supports.

4. Carbon-steel or 304 clips in chemical splash corrode galvanically; the clip becomes the failure point.

A corroded clip snaps under foot traffic, shifting the panel and creating a trip hazard. Carbon-steel clips in acid mists fail in 6-12 months.

Use SS316 clips exclusively. Torque to 5 N m max; over-torque cracks the bar. Inspect clips each turnaround and replace any with pitting.

Failure mode Trigger condition Prevention parameters
Resin swelling Solvent/acid splash on wrong resin Vinyl ester; resistance chart; media+temp match
Static ignition Non-conductive panel in Zone 1/2 Conductive grating <10^6 ohm; SS316 earthing 3 m
Over-span deflection Bearing centres >900 mm on 38 mm m38 rating; 50 mm at 1200 mm; intermediate supports
Clip corrosion Carbon/304 clips in acid mist SS316 only; 5 N m torque; annual pitting check

Related product family and further reading

This case sits inside the molded 38 mm FRP grating family (vinyl ester resin, grit top), supported by the matching pultruded FRP profiles for frames and handrails, the SS316 clip range, and custom cutting for irregular openings. For longer spans or higher loads the same resin system is also available as pultruded grating and as FRP plate. The links below open the product pages and the adjacent case studies on this site.

Document Preview

Preview mode · For full document, click Download

Download Document

Thank you for your interest. Please fill in your email and company name. Our technical and sales team will contact you within 30 minutes (during working hours) to provide support!

📧 Your information will be sent to sales@gratingfrp.com. We respect your privacy and will never share your data.

Thank You!

Your request has been received successfully.

Our technical and sales team will contact you within 30 minutes (during working hours) to provide the document and professional support!

If you need urgent assistance, please email: sales@gratingfrp.com